Inconel • Hastelloy • Nickel-Based Alloys
Nickel Alloys & Superalloys
Inconel and Hastelloy supplier in Turkey through international sourcing. High-performance nickel-based alloys for applications operating under high temperature, corrosion and mechanical load. International sourcing according to specification and quantity.
01
Overview
Nickel alloys are alloys in which nickel is the main element or, together with iron, forms the basis of the structure; additions of chromium, molybdenum, iron, copper, cobalt, niobium, titanium and aluminium produce different property profiles. They are broadly classified as corrosion-resistant alloys (Ni-Cr-Mo, Ni-Mo, Ni-Cu), high-temperature alloys (Ni-Cr, Ni-Fe-Cr), age-hardenable superalloys and controlled-expansion alloys. Their austenitic structure retains toughness at low and high temperatures; superalloys gain high-temperature strength through γ′ and γ″ precipitates. Selection weighs service temperature, environment (oxidising or reducing, chlorides, H₂S), load and duration, together with the applicable specification.
- Ni-Cr-Mo (625, C-276, C-22): resistance to pitting and crevice corrosion in chloride and acidic media
- Ni-Mo (B-2, B-3): corrosion resistance in reducing acids such as hydrochloric acid
- Ni-Cu (400, K-500): seawater and hydrofluoric acid environments
- Age-hardenable (718, X-750, Waspaloy): high-temperature strength through γ′ / γ″ precipitates
- Ni-Fe-Cr (800H, 825): high-temperature and general corrosion service with lower nickel content
- Invar 36 and Kovar: controlled thermal expansion
02
Material Grades
02.1
Inconel Alloys
Nickel-chromium alloys (600, 601, 625, 718, X-750 etc.); strength, oxidation and corrosion resistance at high temperature. Selection depends on temperature, load, duration and environment.
Typical applicationsGas turbine and engine parts, heat-treatment furnace equipment, aerospace, energy and chemical processing.

Alloy 625 (Inconel 625) Nickel Alloy
Available on Request
2.4856·NiCr22Mo9Nb·N06625
Alloy 625 (2.4856) is a Ni-Cr alloy that gains its strength from the solid-solution effect of Mo and Nb and is not hardenable by heat treatment. Usable from cryogenic temperatures up to 980 °C, it is chosen for marine, chemical and flue-gas equipment and as a welding filler.
Alloy 718 (Inconel 718) Nickel Alloy
Available on Request
2.4668·NiCr19Fe19Nb5Mo3·N07718
Alloy 718 (2.4668) is a Ni-Cr-Fe superalloy age-hardened through Nb, Ti and Al, reaching Rm ≈ 1300–1450 MPa after solution treatment and ageing. Its slow ageing response eases welding; it is used up to 650 °C in turbine, rocket-engine and well equipment.
Alloy 600 (Inconel 600) Nickel Alloy
Available on Request
N06600·2.4816·NiCr15Fe
A non-age-hardenable Ni-Cr-Fe alloy with at least 72 % nickel and 14–17 % chromium. Its resistance to oxidation up to 1150 °C, chloride SCC and caustic media leads to use in furnace muffles, nuclear steam-generator tubing and chemical plant.
Alloy 601 (Inconel 601) Nickel Alloy
Available on Request
N06601·2.4851·NiCr23Fe
A Ni-Cr-Fe alloy with 21–25 % chromium and 1.0–1.7 % aluminium whose oxide scale stays adherent under thermal cycling. Suited to heat-treatment baskets, radiant tubes and petrochemical furnace parts in service to 1200 °C.
Alloy X-750 (Inconel X-750) Nickel Alloy
Available on Request
N07750·2.4669·NiCr15Fe7TiAl
Nickel-chromium alloy age-hardened through titanium, aluminium and niobium. After ageing it reaches 1100–1300 MPa with relaxation resistance up to 700 °C, so it is chosen for high-temperature springs, gas-turbine bolts and nuclear reactor internals.
Alloy 690 (Inconel 690) Nickel-Chromium-Iron Alloy
Available on Request
N06690·2.4642·NiCr29Fe
Alloy 690 (2.4642) is a non-hardenable Ni-Cr-Fe alloy with 27–31 % chromium. The high chromium level gives resistance to oxidising acids, high-temperature sulphur-bearing gases and stress corrosion cracking in high-temperature water. It is used for nuclear steam generator tubing, nitric acid equipment and thermal process parts, and is supplied annealed.
Alloy 706 (Inconel 706) Nickel-Iron-Chromium Superalloy
Available on Request
N09706·Inconel 706
Alloy 706 is a Ni-Fe-Cr superalloy age-hardened through Nb and Ti; its chemistry is close to Alloy 718 with a higher iron content. It stands out for producibility in large forged sections and easier machining than 718. It is used for land-based gas turbine discs, shafts and rings, and is supplied solution treated or aged.
Alloy 725 (Inconel 725) Nickel Alloy
Available on Request
N07725·Inconel 725
Alloy 725 takes a Ni-Cr-Mo-Nb chemistry close to Alloy 625 and adds titanium to make it age-hardenable. Its corrosion resistance is close to that of 625, while ageing roughly doubles the yield strength. It is used for hangers, nipples and fasteners in H2S-bearing sour gas wells (NACE MR0175) and is supplied solution treated + aged.
02.2
Hastelloy Alloys
Nickel-molybdenum and nickel-chromium-molybdenum alloys (C-276, C-22, C-4, B-2, B-3) provide corrosion resistance in acidic and chloride environments; oxidising versus reducing conditions drive the selection. Hastelloy X (Ni-Cr-Fe-Mo) is used for oxidation resistance and strength at high temperature.
Typical applicationsChemical and petrochemical processing, flue gas desulphurisation, acid production, heat exchangers; gas turbine combustor and furnace parts for Hastelloy X.

Alloy C-276 (Hastelloy C-276) Nickel Alloy
Available on Request
2.4819·NiMo16Cr15W·N10276
Alloy C-276 (2.4819) is a nickel alloy with 15–17 % Mo, 14.5–16.5 % Cr and 3–4.5 % W; its carbon limit of ≤0.01 restricts intergranular attack in weld zones. It is used for reactors, FGD systems and bleaching equipment where oxidising and reducing media occur together.
Alloy C-22 (Hastelloy C-22) Nickel Alloy
Available on Request
N06022·2.4602·NiCr21Mo14W
Nickel alloy with chromium, molybdenum and tungsten and carbon limited to 0.015 %. Withstands both oxidising and reducing chemicals and localised attack in chloride solutions, including the weld heat-affected zone; used in flue-gas desulphurisation and chemical process equipment.
Alloy B-2 (Hastelloy B-2) Nickel-Molybdenum Alloy
Available on Request
N10665·2.4617·NiMo28
Nickel-molybdenum alloy with 26–30 % Mo and low chromium and iron. Used for reactors, columns, valves and storage equipment handling reducing acids such as HCl, H2SO4 and H3PO4; not suitable for oxidising conditions.
Alloy C-4 (Hastelloy C-4) Nickel-Chromium-Molybdenum Alloy
Available on Request
N06455·2.4610·NiMo16Cr16Ti
Alloy C-4 (2.4610) is a titanium-stabilised Ni-Cr-Mo alloy with 14–18 % Cr and 14–17 % Mo. Its thermal stability against phase precipitation at 650–1040 °C limits intergranular attack in parts that cannot be solution annealed after welding or hot forming. It is used for chemical process, pickling and flue gas cleaning equipment and is supplied solution annealed.
Alloy B-3 (Hastelloy B-3) Nickel-Molybdenum Alloy
Available on Request
N10675·2.4600·NiMo29Cr
Alloy B-3 (2.4600) is a nickel-molybdenum alloy with 27–32 % Mo; adjusted chromium and iron levels give it better thermal stability at intermediate temperatures than B-2. This reduces the tendency to embrittle during fabrication and welding. It is used in reducing acids such as HCl, H2SO4 and H3PO4, is not suited to oxidising conditions, and is supplied solution annealed.
Alloy X (Hastelloy X) Nickel-Chromium-Iron-Molybdenum Alloy
Available on Request
N06002·2.4665·NiCr22Fe18Mo
Alloy X (2.4665) is a non-hardenable Ni-Cr-Fe-Mo high-temperature alloy. It combines solid-solution strength with oxidation resistance up to about 1200 °C and is readily formed and welded as sheet and plate. It is used for gas turbine combustors, transition ducts and furnace parts, and is supplied solution treated.
02.3
Monel Alloys
Nickel-copper alloys (400, K-500); corrosion resistance in seawater and many acid environments. K-500 offers higher strength through age hardening.
Typical applicationsMarine applications, pump shafts, valve parts, chemical equipment, fasteners.

Alloy 400 (Monel 400) Nickel-Copper Alloy
Available on Request
2.4360·NiCu30Fe·N04400
Alloy 400 (2.4360) consists of at least 63 % nickel and 28–34 % copper and gains strength through cold work rather than heat treatment. It is used for pumps, valves, shafts, exchanger tubes and fasteners in contact with seawater, hydrofluoric acid or alkalis.
Alloy K-500 (Monel K-500) Nickel-Copper Alloy
Available on Request
N05500·2.4375·NiCu30Al
Nickel-copper alloy that becomes age-hardenable through aluminium and titanium. After ageing it reaches 950–1100 MPa tensile strength while keeping seawater resistance at the Alloy 400 level; used for pump shafts, subsea bolting and downhole tools.
02.4
Other Nickel Alloys & Superalloys
Incoloy 800H and 825, Nimonic 80A, Waspaloy, commercially pure nickel (Alloy 200) and the controlled-expansion alloys Invar 36 and Kovar.
Typical applicationsHigh-temperature and turbine parts, petrochemical, electronics and precision measurement applications.

Alloy 800H / 800HT (Incoloy) Nickel-Iron-Chromium Alloy
Available on Request
N08810 / N08811·1.4958 / 1.4959·X5NiCrAlTi31-20
An iron-nickel-chromium alloy with carbon held at 0.05–0.10 % and controlled grain size. Creep strength at 600–1000 °C and ASME pressure-equipment approval lead to its use in superheater and reformer tubing and high-temperature heat exchangers.
Alloy 825 (Incoloy 825) Nickel-Iron-Chromium Alloy
Available on Request
N08825·2.4858·NiCr21Mo
A nickel-iron-chromium base alloyed with copper, molybdenum and titanium. Its resistance to sulphuric and phosphoric acids, chloride SCC and H2S-bearing sour service (NACE MR0175) leads to use in downhole tubing, pickling equipment and chemical process plant.
Waspaloy Nickel-Base Superalloy
Available on Request
N07001·2.4654·NiCr19Co14Mo4Ti
Waspaloy (2.4654) is a nickel-base superalloy with 12–15 % cobalt and 3.5–5 % molybdenum, age-hardened by Ti and Al. It is used for turbine discs, rings and fasteners that need creep and rupture strength up to 760 °C, beyond the temperature range of Alloy 718.
Nimonic 80A Nickel-Chromium Superalloy
Available on Request
N07080·2.4952·NiCr20TiAl
Nimonic 80A (2.4952) is a nickel alloy with 18–21 % chromium, age-hardened by additions of 1.8–2.7 % Ti and 1.0–1.8 % Al. It is used for engine exhaust valves, turbine blades and high-temperature bolting that must resist creep and stress relaxation up to 815 °C.
Nickel 200 / 201 Commercially Pure Nickel
Available on Request
N02200 / N02201·2.4066 / 2.4068·Ni 99.2 / LC-Ni 99
Commercially pure nickel with at least 99 % Ni; grade 201, with reduced carbon, is selected for service above 315 °C. Resistant to caustic soda and alkalis and a good conductor of heat and electricity, it is used in caustic plants, food processing and electronic parts.
Invar 36 Low-Expansion Nickel-Iron Alloy
Available on Request
K93600 / K93603·1.3912·Ni36
Invar 36 (1.3912) is an iron-nickel alloy with 35–37 % nickel and a very low thermal expansion of ≈ 1.3 ×10⁻⁶/K between 20 and 100 °C. It is used where parts must hold their dimensions through temperature changes: composite tooling, measuring instruments, optical benches and LNG lines.
Kovar (ASTM F15) Glass-Sealing Nickel-Cobalt-Iron Alloy
Available on Request
K94610·1.3981·NiCo29-18
Kovar (ASTM F15) is an iron-based alloy with about 29 % Ni and 17 % Co whose thermal expansion is controlled to match hard (borosilicate) glasses and alumina ceramics. It is used for hermetic seals in electronic package housings, glass-to-metal feedthroughs and vacuum tubes.
Alloy 20 (Carpenter 20Cb-3) Nickel-Iron-Chromium Alloy
Available on Request
N08020·2.4660·NiCr20CuMo
Alloy 20 (2.4660, Carpenter 20Cb-3) is a niobium-stabilised Ni-Fe-Cr alloy containing copper and molybdenum. Developed for sulphuric acid service, it offers higher resistance to chloride SCC and post-weld intergranular attack than austenitic stainless steels. It is used for acid pickling, chemical and food process equipment and is supplied in the stabilised annealed condition.
03
Chemical Composition
| Grade | Ni | Cr | Mo | Fe | Co | Cu | Nb+Ta | Ti | Al |
|---|---|---|---|---|---|---|---|---|---|
| Inconel Alloys | |||||||||
| Alloy 625 (Inconel 625) Nickel Alloy | ≥58.0 | 20.0–23.0 | 8.0–10.0 | ≤5.0 | — | — | 3.15–4.15 | ≤0.40 | ≤0.40 |
| Alloy 718 (Inconel 718) Nickel Alloy | 50.0–55.0 | 17.0–21.0 | 2.80–3.30 | balance | — | — | 4.75–5.50 | 0.65–1.15 | 0.20–0.80 |
| Alloy 600 (Inconel 600) Nickel Alloy | ≥72.0 | 14.0–17.0 | — | 6.0–10.0 | — | — | — | — | — |
| Alloy 601 (Inconel 601) Nickel Alloy | 58.0–63.0 | 21.0–25.0 | — | balance | — | — | — | — | 1.00–1.70 |
| Alloy X-750 (Inconel X-750) Nickel Alloy | ≥70.0 | 14.0–17.0 | — | 5.0–9.0 | — | — | 0.70–1.20 | 2.25–2.75 | 0.40–1.00 |
| Alloy 690 (Inconel 690) Nickel-Chromium-Iron Alloy | ≥58.0 | 27.0–31.0 | — | 7.0–11.0 | — | ≤0.50 | — | — | — |
| Alloy 706 (Inconel 706) Nickel-Iron-Chromium Superalloy | 39.0–44.0 | 14.5–17.5 | — | balance | — | — | 2.5–3.3 | 1.5–2.0 | ≤0.40 |
| Alloy 725 (Inconel 725) Nickel Alloy | 55.0–59.0 | 19.0–22.5 | 7.0–9.5 | balance | — | — | 2.75–4.0 | 1.0–1.7 | ≤0.35 |
| Hastelloy Alloys | |||||||||
| Alloy C-276 (Hastelloy C-276) Nickel Alloy | balance | 14.5–16.5 | 15.0–17.0 | 4.0–7.0 | ≤2.5 | — | — | — | — |
| Alloy C-22 (Hastelloy C-22) Nickel Alloy | balance | 20.0–22.5 | 12.5–14.5 | 2.0–6.0 | ≤2.5 | — | — | — | — |
| Alloy B-2 (Hastelloy B-2) Nickel-Molybdenum Alloy | balance | ≤1.0 | 26.0–30.0 | ≤2.0 | ≤1.0 | — | — | — | — |
| Alloy C-4 (Hastelloy C-4) Nickel-Chromium-Molybdenum Alloy | balance | 14.0–18.0 | 14.0–17.0 | ≤3.0 | ≤2.0 | — | — | ≤0.70 | — |
| Alloy B-3 (Hastelloy B-3) Nickel-Molybdenum Alloy | ≥65.0 | 1.0–3.0 | 27.0–32.0 | 1.0–3.0 | — | — | — | — | — |
| Alloy X (Hastelloy X) Nickel-Chromium-Iron-Molybdenum Alloy | balance | 20.5–23.0 | 8.0–10.0 | 17.0–20.0 | 0.50–2.50 | — | — | — | — |
| Monel Alloys | |||||||||
| Alloy 400 (Monel 400) Nickel-Copper Alloy | ≥63.0 | — | — | ≤2.5 | — | 28.0–34.0 | — | — | — |
| Alloy K-500 (Monel K-500) Nickel-Copper Alloy | ≥63.0 | — | — | ≤2.0 | — | 27.0–33.0 | — | 0.35–0.85 | 2.30–3.15 |
| Other Nickel Alloys & Superalloys | |||||||||
| Alloy 800H / 800HT (Incoloy) Nickel-Iron-Chromium Alloy | 30.0–35.0 | 19.0–23.0 | — | ≥39.5 | — | — | — | — | — |
| Alloy 825 (Incoloy 825) Nickel-Iron-Chromium Alloy | 38.0–46.0 | 19.5–23.5 | 2.5–3.5 | ≥22.0 | — | 1.5–3.0 | — | 0.6–1.2 | — |
| Waspaloy Nickel-Base Superalloy | balance | 18.0–21.0 | 3.5–5.0 | ≤2.0 | 12.0–15.0 | — | — | 2.75–3.25 | 1.20–1.60 |
| Nimonic 80A Nickel-Chromium Superalloy | balance | 18.0–21.0 | — | ≤3.0 | ≤2.0 | — | — | 1.80–2.70 | 1.00–1.80 |
| Nickel 200 / 201 Commercially Pure Nickel | ≥99.0 | — | — | ≤0.40 | — | ≤0.25 | — | — | — |
| Invar 36 Low-Expansion Nickel-Iron Alloy | 35.0–37.0 | — | — | balance | — | — | — | — | — |
| Kovar (ASTM F15) Glass-Sealing Nickel-Cobalt-Iron Alloy | 29.0 | — | — | balance | 17.0 | — | — | — | — |
| Alloy 20 (Carpenter 20Cb-3) Nickel-Iron-Chromium Alloy | 32.0–38.0 | 19.0–21.0 | 2.0–3.0 | balance | — | 3.0–4.0 | 8×C–1.00 | — | — |
Values in wt. %; ranges per each grade’s reference standard. The full list and reference standard are on the grade page. The analysis on the material certificate governs on delivery.
04
Mechanical Properties
Values for bar products are minimum (≥) values from the relevant ASTM / AMS specifications or typical (≈) values; they vary with delivery and heat-treatment condition and section size. For age-hardenable alloys, values depend on the solution and ageing cycle applied.
| Grade | Condition | Tensile strength Rm (MPa) | Yield strength Rp0.2 (MPa) | Elongation A (%) | Hardness |
|---|---|---|---|---|---|
| Alloy 600 | Annealed (ASTM B166) | ≥ 550 | ≥ 240 | ≥ 30 | — |
| Alloy 625 | Annealed, Grade 1 (ASTM B446, ≤ 100 mm) | ≥ 827 | ≥ 414 | ≥ 30 | — |
| Alloy 718 | Solution treated + aged (AMS 5663) | ≥ 1275 | ≥ 1034 | ≥ 12 | ≈ 40–45 HRC |
| Alloy C-276 | Solution annealed (ASTM B574) | ≥ 690 | ≥ 283 | ≥ 40 | — |
| Alloy C-22 | Annealed (ASTM B574) | ≥ 690 | ≥ 310 | ≥ 45 | — |
| Alloy 400 | Annealed (ASTM B164) | ≥ 483 | ≥ 172 | ≥ 35 | — |
| Alloy K-500 | Aged (typical) | ≈ 950–1100 | — | — | ≈ 27–35 HRC |
| Alloy 825 | Annealed (ASTM B425) | ≥ 586 | ≥ 241 | ≥ 30 | — |
| Alloy 800H / 800HT | Solution annealed (ASTM B408) | ≥ 448 | ≥ 172 | ≥ 30 | — |
| Waspaloy | Solution treated + stabilised + aged (typical) | ≈ 1250–1400 | — | — | ≈ 36–42 HRC |
For information only. Sheet, plate, tube and forgings are covered by different specifications and values. The applicable specification and material certificate govern every order.
05
Physical Properties
Approximate room-temperature values; representative grades are shown to illustrate the differences between alloy families.
| Grade / group | Density (g/cm³) | Modulus of elasticity (GPa) | Thermal conductivity (W/m·K) | Thermal expansion coefficient (10⁻⁶/K, 20–100 °C) |
|---|---|---|---|---|
| Alloy 600 | 8.47 | 207 | 14.9 | 13.3 |
| Alloy 625 | 8.44 | 207 | 9.8 | 12.8 |
| Alloy 718 | 8.19 | 200 | 11.4 | 13.0 |
| Alloy C-276 | 8.89 | 205 | ≈ 10 | 11.2 |
| Alloy 400 | 8.80 | 180 | 21.8 | 13.9 |
| Alloy 825 | 8.14 | 196 | 11.1 | 14.0 |
| Invar 36 | 8.1 | 141 | ≈ 10 | ≈ 1.3 |
Values are approximate; thermal expansion values refer to roughly 20–100 °C. Use producer data and the material certificate for design calculations.
06
Applications
- Aerospace: gas turbine discs, shafts, blades and fasteners (718, Waspaloy)
- Energy: turbine parts, heat exchangers and steam generator tubing (690)
- Chemical and petrochemical: reactors, columns and piping (C-276, C-22, 825)
- Oil and gas: downhole equipment, valves and fasteners (718, 725, 625)
- Marine: pump shafts, valve parts and seawater equipment (400, K-500)
- Heat treatment and furnace equipment: muffles, baskets and radiant tubes (600, 601, 800H)
- Environmental technology: flue gas desulphurisation and acid production (C-276, C-22)
- Electronics and precision measurement: glass-to-metal seals and low-expansion parts (Kovar, Invar 36)
- Defense: components requiring high-temperature and corrosion resistance
07
Product Forms & Delivery Conditions
Product forms
- Round bar
- Plate
- Sheet
- Tube
- Forgings
Availability depends on alloy, specification and quantity.
Delivery conditions
- Annealed — e.g. Alloy 600, 625 Grade 1, 400, 825
- Solution annealed — e.g. C-276, 625 Grade 2, 800H / 800HT
- Solution treated, ready for ageing — e.g. 718, X-750, Waspaloy, K-500
- Solution treated + aged (e.g. AMS 5663)
- Stress relieved (upon request)
- Hot rolled or forged, cold drawn; peeled or ground surface
08
Applicable Standards & Certification
Product standards and specifications
- ASTM B166 — Ni-Cr-Fe alloys (600, 601, 690) rod, bar and wire
- ASTM B446 — Ni-Cr-Mo-Nb alloy (625) rod and bar
- ASTM B637 — Precipitation-hardening nickel alloy bars and forgings (718, X-750, Waspaloy)
- ASTM B574 / B335 — Ni-Cr-Mo (C-276, C-22, C-4) and Ni-Mo (B-2, B-3) rod
- ASTM B164 / B865 — Ni-Cu alloys (400 / K-500) rod and bar
- ASTM B408 / B425 — Ni-Fe-Cr (800H) and Ni-Fe-Cr-Mo-Cu (825) rod and bar
- ASTM B168 / B443 / B575 — 600, 625 and Ni-Cr-Mo alloys plate, sheet and strip
- AMS 5662 / AMS 5663 — Alloy 718 bars and forgings (solution treated / aged)
- AMS 5666 (625), AMS 5667 (X-750), AMS 5706 / 5707 (Waspaloy) — aerospace specifications
- NACE MR0175 / ISO 15156 — Material requirements for H₂S-containing oil and gas environments
Certification and inspection documents
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. ASTM E2375), upon request
- Intergranular corrosion testing (e.g. ASTM G28)
- Grain size report (ASTM E112)
- PMI (positive material identification)
- Heat-treatment report, tensile and hardness test results
A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.
Hard-to-find nickel alloys?
Send us your specification and quantity. We review grade, standard, dimensions, heat-treatment condition, testing and certification requirements together and identify suitable options through our international supplier network.
Material Availability & Supply Capability
Move Metal is not a producer; we focus on technical supply and international sourcing. The supply status of each grade is shown with the statuses below; a grade listed on the site does not mean it is held in stock.
- Regular Supply
- Materials with an established supply relationship, available for recurring requirements.
- Available on Request
- Materials sourced on request through our international producer and supplier network.
- Special Sourcing
- Requirements calling for special dimensions, certification or producer approval, sourced individually.
- Under Development
- Materials we are working to bring into our supply scope.
Please Include
- Alloy (with UNS or W.Nr.)
- Standard and specification (e.g. ASTM B446, AMS 5662)
- Dimensions and tolerance
- Heat-treatment condition (annealed, solution treated, aged)
- Testing requirements
- Certification
- Origin
- Quantity
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.