Skip to content

Invar 36 Low-Expansion Nickel-Iron Alloy

Invar 36

Available on Request

  • UNSK93600 / K93603
  • EN1.3912
  • ENNi36
  • ASTMF1684
  • TicariInvar, Nilo 36, Pernifer 36

Invar 36 (1.3912) is an iron-nickel alloy with 35–37 % nickel and a very low thermal expansion of ≈ 1.3 ×10⁻⁶/K between 20 and 100 °C. It is used where parts must hold their dimensions through temperature changes: composite tooling, measuring instruments, optical benches and LNG lines.

Spectral Analysis

wt. % · ASTM F1684 ranges
Ni
35.0–37.0
Fe
balance
Mn
≤0.60
Si
≤0.35
C
≤0.05

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Very low thermal expansion (≈ 1.3 ×10⁻⁶/K, 20–100 °C)
  • Dimensional stability (with stabilising treatment)
  • Toughness at cryogenic temperatures
  • Ferromagnetic
  • Good machinability and weldability
  • Moderate strength (Rm ≈ 450–550 MPa)

02Applications

  • Composite (carbon fibre) tooling and fixtures
  • Precision instruments and pendulums
  • LNG tanks and pipelines
  • Optical and laser benches
  • Electronic and CRT components

03Delivery Condition

  • Annealed or stabilised; plate, bar, sheet, forging (ASTM F1684).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Soft annealingTemperatureTime →800–850 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Is there a better material?

Grades in the same material family as Invar 36 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Invar 36 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than Invar 36 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

07Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Invar 36 Quotation

Not sure if Invar 36 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote