Skip to content

Waspaloy Nickel-Base Superalloy

Waspaloy

Available on Request

  • UNSN07001
  • EN2.4654
  • ENNiCr19Co14Mo4Ti
  • AMS5704 / 5706 / 5707

Waspaloy (2.4654) is a nickel-base superalloy with 12–15 % cobalt and 3.5–5 % molybdenum, age-hardened by Ti and Al. It is used for turbine discs, rings and fasteners that need creep and rupture strength up to 760 °C, beyond the temperature range of Alloy 718.

Spectral Analysis

wt. % · AMS 5706 ranges
Ni
balance
Cr
18.0–21.0
Co
12.0–15.0
Mo
3.5–5.0
Ti
2.75–3.25
Al
1.20–1.60
Fe
≤2.0
C
0.02–0.10

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • High creep and rupture strength up to 760 °C
  • Rm 1250–1400 MPa after ageing
  • Oxidation resistance up to 870 °C
  • Higher temperature capability than Alloy 718
  • Fatigue strength with controlled grain size
  • AMS / aerospace certification

02Applications

  • Gas turbine discs and rings
  • Turbine blades, seals and casings
  • Combustor components
  • High-temperature fasteners
  • Rocket engine components

03Delivery Condition

  • Solution treated or fully heat treated; bar, forging, ring, plate (AMS 5704 / 5706 / 5707 / 5544).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →~1080 °C
AgeingTemperatureTime →~845 °C
Stages and temperatures are typical values; soaking times depend on section size.

Ageing Diagram

700 °C → 39 HRC730 °C → 40 HRC760 °C → 41 HRC790 °C → 40 HRC820 °C → 38 HRC850 °C → 35 HRC01002003004005006007008009003035404550Ageing temperature [°C]Hardness [HRC]
Hardness versus ageing temperature after solution treatment and stabilisation (approximate).

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Is there a better material?

Grades in the same material family as Waspaloy with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Waspaloy without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

07Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Waspaloy Quotation

Not sure if Waspaloy is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote