Skip to content

Alloy 20 (Carpenter 20Cb-3) Nickel-Iron-Chromium Alloy

Alloy 20

Available on Request

  • UNSN08020
  • EN2.4660
  • ENNiCr20CuMo
  • TicariCarpenter 20Cb-3

Alloy 20 (2.4660, Carpenter 20Cb-3) is a niobium-stabilised Ni-Fe-Cr alloy containing copper and molybdenum. Developed for sulphuric acid service, it offers higher resistance to chloride SCC and post-weld intergranular attack than austenitic stainless steels. It is used for acid pickling, chemical and food process equipment and is supplied in the stabilised annealed condition.

Spectral Analysis

wt. % · ASTM B473 ranges
Ni
32.0–38.0
Cr
19.0–21.0
Cu
3.0–4.0
Mo
2.0–3.0
Nb+Ta
8×C–1.00
Fe
balance
Mn
≤2.0
Si
≤1.0
C
≤0.07

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Resistance in sulphuric acid over a wide range of concentrations and temperatures
  • Resistance to chloride SCC
  • Niobium-stabilised: intergranular corrosion resistance after welding
  • Rm ≈ 550–650 MPa, Rp0.2 ≈ 240–350 MPa (annealed, typical)
  • Good formability and weldability
  • Not hardenable by heat treatment

02Applications

  • Sulphuric acid pickling tanks, racks and heating coils
  • Chemical process vessels, piping and heat exchangers
  • Pump, valve and fitting parts
  • Food, pharmaceutical and solvent production equipment
  • Synthetic rubber and plastics production equipment

03Delivery Condition

  • Stabilised annealed; bar, plate, sheet, tube (ASTM B473 / B463 / B729).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Soft annealingTemperatureTime →925–1010 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Is there a better material?

Grades in the same material family as Alloy 20 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Alloy 20 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than Alloy 20 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

07Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Alloy 20 Quotation

Not sure if Alloy 20 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote