Alloy 600 (Inconel 600) Nickel Alloy

Alloy 600

Available on Request

  • UNSN06600
  • EN2.4816
  • ENNiCr15Fe
  • TicariInconel 600

A non-age-hardenable Ni-Cr-Fe alloy with at least 72 % nickel and 14–17 % chromium. Its resistance to oxidation up to 1150 °C, chloride SCC and caustic media leads to use in furnace muffles, nuclear steam-generator tubing and chemical plant.

Spectral Analysis

wt. % · ASTM B166 ranges
Ni
≥72.0
Cr
14.0–17.0
Fe
6.0–10.0
Mn
≤1.00
C
≤0.15
Si
≤0.50

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Oxidation resistance up to 1150 °C
  • High resistance to chloride SCC
  • Very good resistance in caustic media
  • Good formability and weldability
  • Not hardenable by heat treatment
  • Toughness down to −200 °C

02Applications

  • Furnace muffles, retorts, heat-treatment fixtures
  • Chemical process equipment (caustic, organic chlorides)
  • Nuclear steam generator tubing
  • Gas turbine components
  • Food and paper industry equipment

03Delivery Condition

  • Annealed; bar, plate, sheet, tube, forging (ASTM B166 / B168 / B167).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Soft annealingTemperatureTime →950–1050 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Mechanical Properties

Values by delivery condition; actual values depend on product form, section size and amount of cold work.

ConditionRm (MPa)Rp0.2 (MPa)A (%)HardnessBasis / note
Annealed (rod, bar)≥ 552≥ 241≥ 30—ASTM B166 min.
Annealed — typical≈ 550–690≈ 205–345≈ 35–55≈ 65–85 HRBRoom temperature
Cold drawn — typical≈ 720–1030≈ 550–860≈ 10–30≈ 90 HRB – 30 HRCDepending on degree of cold work
Stress relieved (870–900 °C)————Values depend on prior cold work; on request

Minimum values apply to the stated standard and condition; typical values (≈) are for guidance. The applicable specification and material certificate govern for orders.

07Applicable Standards & Specifications

  • ASTM B166 — Rod, bar and wire (UNS N06600)
  • ASTM B167 — Seamless pipe and tube
  • ASTM B168 — Plate, sheet and strip
  • ASTM B564 — Forgings
  • ASTM B163 — Condenser and heat-exchanger tubes
  • DIN 17742 — Wrought Ni-Cr alloys, composition (2.4816)
  • NACE MR0175 / ISO 15156 — Sour (H₂S) service (on request)

A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.

08Microstructure & Metallurgical Properties

Typical microstructure information

Alloy 600 is a non-age-hardenable Ni-Cr-Fe solid-solution alloy. In the annealed delivery condition its microstructure typically consists of an FCC austenitic γ matrix with dispersed chromium carbides and titanium carbonitrides.

Typical metallurgical characteristics

  • FCC austenitic γ matrix (solid solution)
  • Chromium carbides and TiN / Ti(C,N) particles
  • Possible grain-boundary carbide precipitation and sensitisation at 540–760 °C
  • Not hardenable by heat treatment; strength increases by cold work
  • Properties influenced by annealing condition and amount of cold work
1.Typical microstructure
In the annealed condition: γ matrix with annealing twins, discrete chromium-rich carbides (mainly M₇C₃) within grains and at grain boundaries, and angular TiN / Ti(C,N) particles.
2.Heat treatment influence
The annealing temperature (950–1050 °C) controls carbide dissolution and grain size. Holding at about 540–760 °C can precipitate chromium carbides at grain boundaries and cause chromium depletion next to them; annealed Alloy 600 and material exposed to this range do not show the same microstructure.
3.Grain structure
Grain size depends on annealing temperature and prior cold work; a coarser grain is preferred where creep strength at high temperature is required, a finer grain for forming and room-temperature strength.
4.Carbide / precipitate distribution
Chromium carbides (M₇C₃, M₂₃C₆) and TiN / Ti(C,N). For nuclear steam-generator tubing a special thermal treatment can be applied to control grain-boundary carbide distribution.
5.Metallographic examination
Batch-specific metallographic examination is available upon request. A microstructure image alone does not prove chemical analysis, mechanical properties or certificate compliance.

Available technical documentation

  • Chemical composition certificate
  • Mechanical test report, where available
  • Heat treatment information, where available
  • Metallographic examination, upon request

Typical microstructure information. Actual microstructure may vary depending on manufacturing route, product form and heat treatment.

09Is there a better material?

Grades in the same material family as Alloy 600 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Alloy 600 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than Alloy 600 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

10Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Alloy 600 Quotation

Not sure if Alloy 600 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote