Skip to content

Alloy 725 (Inconel 725) Nickel Alloy

Alloy 725

Available on Request

  • UNSN07725
  • TicariInconel 725

Alloy 725 takes a Ni-Cr-Mo-Nb chemistry close to Alloy 625 and adds titanium to make it age-hardenable. Its corrosion resistance is close to that of 625, while ageing roughly doubles the yield strength. It is used for hangers, nipples and fasteners in H2S-bearing sour gas wells (NACE MR0175) and is supplied solution treated + aged.

Spectral Analysis

wt. % · UNS N07725 ranges
Ni
55.0–59.0
Cr
19.0–22.5
Mo
7.0–9.5
Nb
2.75–4.0
Ti
1.0–1.7
Al
≤0.35
Fe
balance
C
≤0.03

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • High strength through ageing; corrosion resistance close to Alloy 625
  • Rp0.2 ≈ 830–900 MPa, Rm ≈ 1030–1200 MPa (aged, typical)
  • Suitable for sour gas (H2S) service (NACE MR0175)
  • Resistance to chloride SCC, pitting and crevice corrosion
  • Resistance to hydrogen embrittlement
  • Corrosion resistance in seawater

02Applications

  • Downhole hangers, landing nipples and side-pocket mandrels
  • Fasteners and shafts in sour gas service
  • Offshore and marine fasteners
  • High-strength valve and pump parts

03Delivery Condition

  • Solution treated or solution treated + aged; bar, forgings (ASTM B805).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →~1040 °C
AgeingTemperatureTime →1. age~730 °C2. age~620 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Is there a better material?

Grades in the same material family as Alloy 725 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Alloy 725 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

07Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Alloy 725 Quotation

Not sure if Alloy 725 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote