Nickel-chromium alloy age-hardened through titanium, aluminium and niobium. After ageing it reaches 1100–1300 MPa with relaxation resistance up to 700 °C, so it is chosen for high-temperature springs, gas-turbine bolts and nuclear reactor internals.
Spectral Analysis
wt. % · AMS 5667 ranges- Ni
- ≥70.0
- Cr
- 14.0–17.0
- Fe
- 5.0–9.0
- Ti
- 2.25–2.75
- Al
- 0.40–1.00
- Nb+Ta
- 0.70–1.20
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Rm 1100–1300 MPa after ageing
- Relaxation resistance up to 700 °C
- Toughness at cryogenic temperatures
- Corrosion resistance at the Alloy 600 level
- Non-magnetic
- Formable in the solution-treated condition
02Applications
- High-temperature springs and diaphragms
- Gas turbine blades, rotors, bolts
- Nuclear reactor springs and internals
- Rocket engine fasteners
- Extrusion dies
03Delivery Condition
- Solution treated or solution treated + aged; bar, wire, plate, forging (AMS 5667 / 5671 / 5698).
04Please Include in Your Request
- Standard and delivery condition
- Form and dimensions (bar, plate, sheet, tube, forging)
- Quantity
- Testing and certification (EN 10204 3.1 / 3.2, NACE)
- Origin requirements
05Heat Treatment
Heat Treatment Steps
Ageing Diagram
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
06Is there a better material?
Grades in the same material family as Alloy X-750 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
Our list has no grade with higher wear resistance than Alloy X-750 without a marked trade-off in its other critical properties.
Higher impact resistance (toughness)
- Alloy 625 (Inconel 625) Nickel Alloy
Toughness: High → Very high
Trade-off: High-temperature strength, Strength, Wear resistance
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights07Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Plate
- Sheet
- Tube
- Forgings
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. ASTM E2375), upon request
- Intergranular corrosion testing (e.g. ASTM G28)
- Grain size report (ASTM E112)
Supply status: Available on Request
Request Alloy X-750 QuotationNot sure if Alloy X-750 is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialGrades in the Same Group
Back to GroupTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.