Nickel-copper alloy that becomes age-hardenable through aluminium and titanium. After ageing it reaches 950–1100 MPa tensile strength while keeping seawater resistance at the Alloy 400 level; used for pump shafts, subsea bolting and downhole tools.

Spectral Analysis

wt. % · QQ-N-286 / ASTM B865 ranges
Ni
≥63.0
Cu
27.0–33.0
Al
2.30–3.15
Ti
0.35–0.85
Fe
≤2.0
Mn
≤1.5

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm 950–1100 MPa, ≈ 27–35 HRC after ageing
  • Seawater and acid resistance at the Alloy 400 level
  • Non-magnetic (down to −100 °C)
  • Cryogenic toughness
  • Low galvanic effect with copper alloys
  • Resistance in hydrofluoric acid and caustic

02Applications

  • Pump shafts and impellers (seawater)
  • Subsea and marine fasteners
  • Oil-well survey and drilling tools
  • Valve bodies and stems
  • Doctor blades and scrapers for paper machines

03Delivery Condition

  • Annealed, annealed + aged or cold drawn + aged; bar, wire, forging (ASTM B865, QQ-N-286).

04Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube, forging)
  • Quantity
  • Testing and certification (EN 10204 3.1 / 3.2, NACE)
  • Origin requirements

05Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →~980 °C
AgeingTemperatureTime →~590 °C
Stages and temperatures are typical values; soaking times depend on section size.

Ageing Diagram

540 °C → 33 HRC565 °C → 34 HRC590 °C → 35 HRC620 °C → 33 HRC650 °C → 30 HRC01002003004005006007002530354045Ageing temperature [°C]Hardness [HRC]
Hardness versus ageing temperature after solution treatment (approximate).

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

06Is there a better material?

Grades in the same material family as Alloy K-500 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Alloy K-500 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

07Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Plate
  • Sheet
  • Tube
  • Forgings

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. ASTM E2375), upon request
  • Intergranular corrosion testing (e.g. ASTM G28)
  • Grain size report (ASTM E112)

Supply status: Available on Request

Request Alloy K-500 Quotation

Not sure if Alloy K-500 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote