Skip to content

O1 Tool Steel

1.2510

  • EN1.2510
  • EN100MnCrW4
  • AISIO1

Oil-hardening cold work steel (AISI O1) alloyed with manganese, chromium and tungsten. A low hardening temperature and limited distortion bring it to 58–64 HRC; used for blanking dies, reamers, taps, woodworking knives and gauges.

Spectral Analysis

wt. % · EN ISO 4957 ranges
C
0.90–1.05
Si
0.10–0.40
Mn
1.00–1.20
Cr
0.50–0.70
V
0.05–0.15
W
0.50–0.70

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Oil hardening; low hardening temperature
  • Easy machinability
  • Good edge retention
  • Low distortion
  • Heat treated to 58–64 HRC

02Applications

  • Cutting and punching dies
  • Reamers, taps and hand tools
  • Woodworking knives
  • Gauges and measuring instruments
  • Small plastic molds and mold pins

03Delivery Condition

  • Max. 229 HB, soft annealed.

04Heat Treatment

Heat Treatment Steps

Stress relievingTemperatureTime →600–650 °C
HardeningTemperatureTime →Preheat~625 °CAustenitise790–830 °C

Quench: Oil or 180–220 °C salt bath

TemperingTemperatureTime →1. temper150–300 °C2. temper150–300 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 65 HRC100 °C → 64 HRC150 °C → 63 HRC200 °C → 62 HRC250 °C → 60.5 HRC300 °C → 59 HRC400 °C → 56 HRC500 °C → 51 HRC010020030040050045505560657075Tempering temperature [°C]Hardness [HRC]1.2510Heat treatment: 790–830 °CQuench: Oil or 180–220 °Csalt bath
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as O1 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Block
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, delivery hardness)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Ultrasonic testing (e.g. SEP 1921, EN 10228-3)
  • Microstructure and inclusion rating (e.g. SEP 1614, ASTM E45, EN 10247)
  • Hardness test report (HB / HRC)
Request O1 Quotation

Not sure if O1 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote