Skip to content

1.2767

  • EN1.2767
  • ENX45NiCrMo4

Cold work tool steel with about 4% nickel, combining high hardenability with toughness. Used for thick-sheet cutting and bending tools, scrap shear blades and cold forging dies that work under impact loading.

Spectral Analysis

wt. % · EN ISO 4957 ranges
C
0.40–0.50
Si
0.10–0.40
Mn
0.20–0.50
Cr
1.20–1.50
Mo
0.15–0.35
Ni
3.80–4.30

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • High toughness
  • Nickel-bearing, impact-resistant steel
  • High hardenability
  • Polishable

02Applications

  • Cutlery (fork and spoon) dies
  • Scrap shear blades
  • Cutting and bending of thick sheet
  • Cold forging and forming dies

03Heat Treatment

Heat Treatment Steps

Stress relievingTemperatureTime →550–600 °C
HardeningTemperatureTime →Preheat~625 °CAustenitise840–870 °C

Quench: Oil or air

TemperingTemperatureTime →1. temper150–250 °C2. temper150–250 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 56 HRC100 °C → 55.5 HRC200 °C → 54 HRC300 °C → 51 HRC400 °C → 48 HRC500 °C → 45 HRC550 °C → 42 HRC600 °C → 38 HRC01002003004005006003035404550556065Tempering temperature [°C]Hardness [HRC]1.2767Heat treatment: 840–870 °CQuench: Oil or air
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

04Is there a better material?

Grades in the same material family as 1.2767 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than 1.2767 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

05Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Block
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, delivery hardness)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Ultrasonic testing (e.g. SEP 1921, EN 10228-3)
  • Microstructure and inclusion rating (e.g. SEP 1614, ASTM E45, EN 10247)
  • Hardness test report (HB / HRC)
Request a Quote

Not sure if 1.2767 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote