Grade 23 is the ELI (extra low interstitial) version of Ti-6Al-4V, with tighter oxygen (≤0.13) and iron (≤0.25) limits that give higher fracture toughness and ductility than Grade 5. It is supplied to ASTM F136 for implants and surgical instruments and is also used for cryogenic pressure vessels.
Spectral Analysis
wt. % · ASTM F136 ranges- Ti
- balance
- Al
- 5.50–6.50
- V
- 3.50–4.50
- Fe
- ≤0.25
- O
- ≤0.13
- C
- ≤0.08
- N
- ≤0.05
- H
- ≤0.012
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Higher fracture toughness and ductility than Grade 5
- Rm ≥ 860 MPa (annealed)
- Biocompatibility (ASTM F136)
- Toughness at cryogenic temperatures
- High fatigue strength
02Applications
- Orthopaedic and dental implants
- Surgical instruments
- Aerospace structural parts (damage tolerant)
- Cryogenic pressure vessels
- High-performance sports and racing parts
03Delivery Condition
- Annealed; bar, plate, sheet. ASTM F136 / AMS certified supply on request.
04Heat Treatment
Heat Treatment Steps
Ageing Diagram
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
05Mechanical Properties
Values by heat-treatment condition; standard minimums are shown with their specification, others are typical. Actual values depend on product form, section size and specification.
| Condition | Tensile strength Rm (MPa) | Yield strength Rp0.2 (MPa) | Elongation A (%) | Hardness | Note |
|---|---|---|---|---|---|
| Annealed — implant bar (ASTM F136) | ≥ 860 | ≥ 795 | ≥ 10 | — | Reduction of area ≥ 25 % |
| Annealed — bar (ASTM B348 Grade 23) | ≥ 828 | ≥ 759 | ≥ 10 | — | Industrial use |
| Annealed (typical) | ≈ 900–950 | ≈ 830–880 | ≈ 12–16 | ≈ 30–34 HRC | Standard delivery condition |
| Solution treated + aged (STA) | — | — | — | — | Per specification; conditions defined in the order |
Elastic modulus ≈ 110–114 GPa, density ≈ 4.43 g/cm³. Fracture toughness is higher than Grade 5; the applicable specification and material certificate govern for orders.
06Applicable Standards & Specifications
- ASTM F136 — Wrought Ti-6Al-4V ELI for surgical implants
- ASTM B348 — Titanium and titanium alloy bars and billets (Grade 23)
- ASTM B265 — Titanium and titanium alloy strip, sheet and plate (Grade 23)
- AMS 4930 — Ti-6Al-4V ELI bars, wire, forgings and rings; annealed
- AMS 4907 — Ti-6Al-4V ELI sheet, strip and plate; annealed
- ISO 5832-3 — Implants for surgery; wrought titanium 6-aluminium 4-vanadium alloy
A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.
07Is there a better material?
Grades in the same material family as Grade 23 Titanium with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
- Ti-10V-2Fe-3Al (Ti-10-2-3) Titanium Alloy
Wear resistance: Low · same level, higher carbide volume / hot hardness (wear ranking 30 → 36)
Trade-off: High-temperature strength, Toughness
- Grade 19 Titanium (Ti-3Al-8V-6Cr-4Mo-4Zr)
Wear resistance: Low · same level, higher carbide volume / hot hardness (wear ranking 30 → 37)
Trade-off: High-temperature strength, Toughness
Higher impact resistance (toughness)
Our list has no grade with higher impact resistance (toughness) than Grade 23 Titanium without a marked trade-off in its other critical properties.
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights08Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Flat bar
- Plate
- Sheet
- Tube
- Forgings
- Cut-to-size
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. AMS 2631; class as required)
- Chemical analysis including H, O and N
- Microstructure and alpha case examination
Supply status: Available on Request
Request Grade 23 Titanium QuotationNot sure if Grade 23 Titanium is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.