Ti-10V-2Fe-3Al (Ti-10-2-3) Titanium Alloy
Ti-10V-2Fe-3Al (Ti-10-2-3)
Available on Request
- UNSR56410
- AMS4984 / 4986 / 4987
Ti-10V-2Fe-3Al is a near-beta titanium alloy with 9–11 % V and 1.6–2.2 % Fe; it can be forged at comparatively low temperatures and hardens through thick sections, which suits large forgings. It is used to AMS 4984/4986/4987 for landing-gear and rotor-hub components.
Spectral Analysis
wt. % · AMS 4986 ranges- Ti
- balance
- V
- 9.0–11.0
- Fe
- 1.6–2.2
- Al
- 2.6–3.4
- O
- ≤0.13
- C
- ≤0.05
- N
- ≤0.05
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Typical Standards
- AMS 4984 / 4986 / 4987 (forgings)
- Producer and OEM specifications
- Customer specifications
02Typical Applications
- Landing gear forgings
- Helicopter rotor hubs
- Wing and fuselage attachment forgings
- High-strength fasteners
03Please Include in Your Request
- Standard and delivery condition
- Form and dimensions (bar, plate, sheet, tube)
- Quantity
- Testing and certification requirements
- Origin requirements
04Heat Treatment
Heat Treatment Steps
Ageing Diagram
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
05Is there a better material?
Grades in the same material family as Ti-10-2-3 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
Our list has no grade with higher wear resistance than Ti-10-2-3 without a marked trade-off in its other critical properties.
Higher impact resistance (toughness)
- Grade 5 Titanium (Ti-6Al-4V)
Toughness: Medium → High
- AMS 4928W Titanium
Toughness: Medium → High
Trade-off: Strength
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights06Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Flat bar
- Plate
- Sheet
- Tube
- Forgings
- Cut-to-size
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 inspection certificate (upon request, third party)
- Ultrasonic testing (e.g. AMS 2631; class as required)
- Chemical analysis including H, O and N
- Microstructure and alpha case examination
Supply status: Available on Request
Request Ti-10-2-3 QuotationNot sure if Ti-10-2-3 is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.