Ti-6Al-2Sn-4Zr-2Mo (Ti-6242) Titanium Alloy

Ti-6Al-2Sn-4Zr-2Mo (Ti-6242)

Available on Request

  • UNSR54620
  • AMS4919 / 4975 / 4976
  • ASTMB348 Grade 6242 (R54620)

Ti-6242 is a near-alpha titanium alloy containing Al, Sn, Zr and Mo, designed to retain creep strength at temperatures where Ti-6Al-4V falls short. It is used for compressor discs and blades, engine casings and exhaust parts (AMS 4919/4975/4976).

Spectral Analysis

wt. % · AMS 4976 ranges
Ti
balance
Al
5.5–6.5
Sn
1.8–2.2
Zr
3.6–4.4
Mo
1.8–2.2
Si
≤0.10
O
≤0.15

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Typical Standards

  • AMS 4919 (sheet/plate), AMS 4975 / 4976 (bar, forging)
  • ASTM B348 (R54620)
  • Customer specifications

02Typical Applications

  • Gas turbine compressor discs and blades
  • Engine casings and exhaust parts
  • High-temperature aerospace structures
  • Racing engine components

03Please Include in Your Request

  • Standard and delivery condition
  • Form and dimensions (bar, plate, sheet, tube)
  • Quantity
  • Testing and certification requirements
  • Origin requirements

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →955–985 °C
AgeingTemperatureTime →~595 °C
Stages and temperatures are typical values; soaking times depend on section size.

Ageing Diagram

540 °C → 38 HRC595 °C → 37 HRC650 °C → 35 HRC700 °C → 33 HRC01002003004005006007002530354045Ageing temperature [°C]Hardness [HRC]Ti-6Al-2Sn-4Zr-2Mo (Ti-6242)Solution treatment: 955–985 °C
Hardness versus stabilisation temperature after solution treatment (≈ 970 °C, air), approximate.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as Ti-6242 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than Ti-6242 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Tube
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. AMS 2631; class as required)
  • Chemical analysis including H, O and N
  • Microstructure and alpha case examination

Supply status: Available on Request

Request Ti-6242 Quotation

Not sure if Ti-6242 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote