Skip to content

34Cr4 Engineering Steel

1.7033

Available on Request

  • EN1.7033
  • EN34Cr4
  • AISI~5132

Chromium alloyed steel for quenching and tempering without molybdenum (1.7033, 34Cr4). Its medium hardenability suits small and medium sections; in the +QT condition it gives 800–950 MPa tensile strength at 16–40 mm. Supplied on request, quenched and tempered or annealed, for shafts, axles, bolts and gears in automotive and machine building.

Spectral Analysis

wt. % · EN ISO 683-2 / EN 10083-3 ranges
C
0.30–0.37
Si
≤0.40
Mn
0.60–0.90
Cr
0.90–1.20

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm 700–1100 MPa (+QT, depending on section)
  • Medium hardenability; for small and medium sections
  • No molybdenum; 34CrMo4 is considered for larger sections
  • Suitable for induction and flame hardening
  • Not suited to welding; if welding is required, preheating and post-weld heat treatment are needed
  • Resulphurised variant 34CrS4 (1.7037) for machining

02Applications

  • Shafts and axles
  • Automotive driveline and steering parts
  • Bolts, studs and nuts (including cold forming)
  • Gears and pinions
  • Connecting rods and links

03Delivery Condition

  • Quenched and tempered (+QT), soft annealed (+A, max. 223 HB) or annealed for cold shearing (+S, max. 255 HB).
  • Resulphurised 34CrS4 (1.7037) can be considered on request.

04Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →Austenitise830–860 °C
TemperingTemperatureTime →540–680 °Cat least 1 h
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Mechanical Properties

Minimum values to EN 10083-3 in the +QT (quenched and tempered) condition by section size; the +A and +S rows give the delivery hardness.

ConditionSection d (mm)Rm (MPa)Rp0.2 min. (MPa)A min. (%)
Soft annealed (+A)AllMax. 223 HB——
Annealed for cold shearing (+S)AllMax. 255 HB——
Quenched and tempered (+QT)d ≤ 16900–110070012
Quenched and tempered (+QT)16 < d ≤ 40800–95059014
Quenched and tempered (+QT)40 < d ≤ 100700–85046015

Values are EN 10083-3 minimums (thickness ranges for flat products differ). Hardenability is limited in larger sections; suitability is assessed before ordering. The applicable specification and material certificate govern for orders.

06Applicable Standards & Specifications

  • EN ISO 683-2 — Alloy steels for quenching and tempering (34Cr4)
  • EN 10083-3 — Steels for quenching and tempering, alloy steels (34Cr4, +A / +S / +QT)
  • EN 10263-4 — Steels for cold heading and cold extrusion, steels for quenching and tempering (34Cr4)
  • DIN 17200 (withdrawn, still used as a reference)

A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.

07Is there a better material?

Grades in the same material family as 34Cr4 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

08Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Peeled bar
  • Ground shafting
  • Hexagon
  • Flat bar
  • Plate
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Tensile and impact (Charpy KV) test report
  • Jominy end-quench test (EN ISO 642) report
  • Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)

Supply status: Available on Request

Request 34Cr4 Quotation

Not sure if 34Cr4 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote