16NiCrMo12 Case-Hardening Steel
16NiCrMo12
Available on Request
- UNI16NiCrMo12
- EN~14NiCrMo13-4 (yakın)
- EN~1.6657 (yakın)
- AFNOR~16NCD13
Case-hardening steel with 2.70–3.20 % nickel, chromium and molybdenum (UNI 7846: 16NiCrMo12). The closest EN grade is 14NiCrMo13-4 (1.6657), but the compositions are not identical. After carburising it combines a hard case with a tough, strong core thanks to its high nickel content; supplied annealed on request for highly loaded gears and rolling elements.
Spectral Analysis
wt. % · UNI 7846 ranges- C
- 0.13–0.19
- Si
- 0.15–0.40
- Mn
- 0.40–0.70
- Cr
- 0.80–1.10
- Mo
- 0.30–0.40
- Ni
- 2.70–3.20
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Surface hardness ≈ 62–64 HRC after carburising (tempering 150–200 °C)
- Core Rm ≈ 980–1520 MPa (depending on section)
- High hardenability; medium and large sections
- Very good core toughness through high nickel
- High surface fatigue (pitting) and impact resistance
- Differs from 14NiCrMo13-4: lower nickel (2.70–3.20 %), higher molybdenum (0.30–0.40 %)
02Applications
- Highly loaded gears and pinions
- Rolling elements and highly loaded bearing parts
- Gearbox and driveline components
- Shafts and pins under impact loading
- Motorsport, defence and heavy machinery driveline parts
03Delivery Condition
- Soft annealed (+A, max. 250 HB) or isothermally annealed (+I, 190–236 HB); bar and forgings.
- Where material is ordered under the UNI name, supply as EN 14NiCrMo13-4 (1.6657) is assessed against composition and specification.
04Heat Treatment
Heat Treatment Steps
Tempering Diagram
If welding is required, it is done in the annealed condition and before carburising, with 150–350 °C preheating. Values are typical (producer data); the applicable specification governs for orders.
05Mechanical Properties
Delivery hardness and test-bar values after core hardening + stress relieving (UNI 7846, reference); core strength depends on section size.
| Condition | Section (mm) | Rm (MPa) | Rp0.2 min. (MPa) | Hardness |
|---|---|---|---|---|
| Soft annealed (+A) | All | — | — | Max. 250 HB |
| Isothermally annealed (+I) | All | — | — | 190–236 HB |
| Core hardened + stress relieved | 11 | 1230–1520 | 980 | 363–432 HB |
| Core hardened + stress relieved | 30 | 1080–1370 | 785 | 327–394 HB |
| Core hardened + stress relieved | 63 | 980–1270 | 735 | 295–373 HB |
| Carburised + hardened + tempered — surface | — | — | — | ≈ 62–64 HRC |
Reference values for UNI 7846 test bars (producer data; the 30 and 63 mm rows are for information). The applicable specification and material certificate govern for orders.
06Applicable Standards & Specifications
- UNI 7846 — Case-hardening steels (16NiCrMo12; former Italian standard, still used as a reference)
- EN 10084 — Case-hardening steels (closest grade 14NiCrMo13-4 / 1.6657; composition not identical)
A product specification and an inspection document are different things: e.g. AMS 4928 is a product specification, EN 10204 3.1 is a type of inspection document; one does not replace the other.
07Is there a better material?
Grades in the same material family as 16NiCrMo12 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
- 34CrAlNi7 Nitriding Steel
Wear resistance: High · same level, higher carbide volume / hot hardness (wear ranking 72 → 78)
Trade-off: Strength, Fatigue resistance, Toughness
Higher impact resistance (toughness)
Our list has no grade with higher impact resistance (toughness) than 16NiCrMo12 without a marked trade-off in its other critical properties.
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights08Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Peeled bar
- Ground shafting
- Hexagon
- Flat bar
- Plate
- Forgings
- Cut to size
Documents and testing
- EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
- EN 10204 3.2 inspection certificate (on request, third party)
- Tensile and impact (Charpy KV) test report
- Jominy end-quench test (EN ISO 642) report
- Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)
Supply status: Available on Request
Request 16NiCrMo12 QuotationNot sure if 16NiCrMo12 is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialTechnical resources for this material
Have a material requirement?
Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.