Skip to content

20NiCrMo2-2 (8620) Case-Hardening Steel

1.6523

Available on Request

  • EN1.6523
  • EN20NiCrMo2-2
  • AISI8620
  • UNSG86200

Case-hardening steel with low nickel, chromium and molybdenum additions (20NiCrMo2-2), equivalent to AISI 8620. After carburising it combines a hard, wear-resistant surface with a tough core. Supplied to specification, soft annealed or +FP, for small and medium-section machine parts such as gears, pinions and shafts.

Spectral Analysis

wt. % · EN 10084 ranges
C
0.17–0.23
Si
≤0.40
Mn
0.65–0.95
Cr
0.35–0.70
Mo
0.15–0.25
Ni
0.40–0.70

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Surface hardness 58–62 HRC after carburising
  • Tough core, good impact resistance
  • Adequate hardenability for small and medium sections
  • Good fatigue strength
  • Good machinability in the annealed condition

02Applications

  • Gears and pinions
  • Shafts, camshafts, pins
  • Bushings and chain parts
  • Automotive and construction-machinery driveline parts
  • Bearing rings (carburised)

03Delivery Condition

  • Soft annealed (+A) or ferrite-pearlite treated (+FP); bar and forgings.

04Heat Treatment

Heat Treatment Steps

CarburisingTemperatureTime →880–980 °C
HardeningTemperatureTime →Austenitise820–860 °C
TemperingTemperatureTime →150–200 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

150 °C → 62 HRC200 °C → 60 HRC250 °C → 58 HRC300 °C → 56 HRC01002003004005055606570Tempering temperature [°C]Hardness [HRC]1.6523Heat treatment: 820–860 °C
Surface hardness after carburising versus tempering temperature (approximate).

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 20NiCrMo2-2 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Peeled bar
  • Ground shafting
  • Hexagon
  • Flat bar
  • Plate
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, mechanical tests)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Tensile and impact (Charpy KV) test report
  • Jominy end-quench test (EN ISO 642) report
  • Ultrasonic testing (e.g. EN 10308 for bars, EN 10228-3 for forgings)

Supply status: Available on Request

Request 20NiCrMo2-2 Quotation

Not sure if 20NiCrMo2-2 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote