Skip to content

H21 Tool Steel

1.2581

  • EN1.2581
  • ENX30WCrV9-3
  • AISIH21

H21-type hot work steel (X30WCrV9-3) with 8.50–9.50 % tungsten. Hot hardness and temper resistance are high; with only moderate toughness it is run preheated and without water quenching, in brass and copper extrusion dies and hot pressing tools.

Spectral Analysis

wt. % · EN ISO 4957 ranges
C
0.25–0.35
Si
0.15–0.50
Mn
0.20–0.50
Cr
2.50–3.20
V
0.30–0.50
W
8.50–9.50

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • High hardness and wear resistance at elevated temperature
  • Very good tempering resistance
  • Moderate toughness; not suitable for sudden water cooling
  • Tools should be preheated before use
  • Heat treated to 48–52 HRC

02Applications

  • Hot extrusion dies for brass and copper
  • Hot pressing and forging die inserts
  • Hot shear blades
  • Mandrels and punches
  • Glass and ceramic mold components

03Delivery Condition

  • Max. 241 HB, soft annealed.

04Heat Treatment

Heat Treatment Steps

Stress relievingTemperatureTime →650–700 °C
HardeningTemperatureTime →1. preheat~650 °C2. preheat~850 °C3. preheat~1050 °CAustenitise1100–1150 °C

Quench: Oil or air/pressurised gas

TemperingTemperatureTime →1. temper600–700 °Cmin. 2 h2. temper600–700 °Cmin. 2 h
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 50 HRC200 °C → 49 HRC300 °C → 48.5 HRC400 °C → 48.5 HRC500 °C → 49.5 HRC550 °C → 50.5 HRC600 °C → 48 HRC650 °C → 45 HRC700 °C → 38 HRC010020030040050060070030354045505560Tempering temperature [°C]Hardness [HRC]1.2581Heat treatment: 1100–1150 °CQuench: Oil orair/pressurised gas
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as H21 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than H21 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Block
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, delivery hardness)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Ultrasonic testing (e.g. SEP 1921, EN 10228-3)
  • Microstructure and inclusion rating (e.g. SEP 1614, ASTM E45, EN 10247)
  • Hardness test report (HB / HRC)
Request H21 Quotation

Not sure if H21 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote