Skip to content

431 Stainless Steel

1.4057

  • EN1.4057
  • ENX17CrNi16-2
  • AISI431

Martensitic stainless steel with 15–17% chromium and 1.5–2.5% nickel; its chromium level is above that of the 13% Cr martensitic grades. Supplied at 30–46 HRC for propeller and pump shafts, bolts and nuts and marine fittings.

Spectral Analysis

wt. % · EN 10088-3 ranges
C
0.12–0.22
Si
≤1.00
Mn
≤1.50
Cr
15.0–17.0
Ni
1.50–2.50

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Applications

  • Bolts and nuts
  • Propeller shafts
  • Pump shafts
  • Mixer rods
  • Marine equipment
  • Laboratory equipment

02Delivery Condition

  • 30–46 HRC

03Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →Preheat~780 °CAustenitise950–1050 °C
TemperingTemperatureTime →1. temper600–700 °C2. temper600–700 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 45 HRC200 °C → 44 HRC300 °C → 43 HRC400 °C → 43 HRC500 °C → 42 HRC600 °C → 34 HRC650 °C → 30 HRC700 °C → 26 HRC01002003004005006007002025303540455055Tempering temperature [°C]Hardness [HRC]1.4057Heat treatment: 950–1050 °C
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

04Is there a better material?

Grades in the same material family as 431 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

05Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
  • Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
  • Detrimental phase testing for duplex steels (ASTM A923)
Request 431 Quotation

Not sure if 431 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote