Skip to content

420 Stainless Steel

1.4021

  • EN1.4021
  • ENX20Cr13
  • AISI420
  • UNSS42000

Martensitic stainless steel with 12–14% chromium and about 0.2% carbon, hardenable to 48–52 HRC. Used annealed or quenched and tempered (+QT800) for shafts, pump and valve parts where moderate resistance to water, steam and weak acids is sufficient.

Spectral Analysis

wt. % · EN 10088-3 ranges
C
0.16–0.25
Si
≤1.00
Mn
≤1.50
Cr
12.0–14.0

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Hardenable by heat treatment (48–52 HRC)
  • Moderate corrosion resistance (water, steam, mild acids)
  • Good strength and wear resistance
  • Magnetic
  • Good machinability in the quenched and tempered condition

02Applications

  • Shafts, pump and valve components
  • Knives, scissors and cutlery
  • Mold components requiring corrosion resistance
  • Turbine and compressor parts
  • Fasteners

03Delivery Condition

  • Annealed max. 230 HB or quenched and tempered (+QT800: 650–850 MPa).

04Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →Preheat~780 °CAustenitise950–1000 °C
TemperingTemperatureTime →1. temper150–250 °C2. temper150–250 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 51 HRC100 °C → 50 HRC200 °C → 49 HRC300 °C → 48 HRC400 °C → 47.5 HRC500 °C → 46 HRC550 °C → 43 HRC600 °C → 35 HRC650 °C → 30 HRC700 °C → 26 HRC0100200300400500600700202530354045505560Tempering temperature [°C]Hardness [HRC]1.4021Heat treatment: 950–1000 °C
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 420 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
  • Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
  • Detrimental phase testing for duplex steels (ASTM A923)
Request 420 Quotation

Not sure if 420 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote