Skip to content

310S Heat-Resistant Stainless Steel

1.4845

Available on Request

  • EN1.4845
  • ENX8CrNi25-21
  • AISI310S
  • UNSS31008

Heat-resistant austenitic stainless steel (310S, UNS S31008) with 24–26 % chromium and 19–22 % nickel. It resists oxidation (scaling) in air up to about 1050 °C and is used for furnace parts, heat-treatment fixtures and combustion-zone equipment. Supplied on request in the solution-annealed condition as bar, sheet, plate and tube.

Spectral Analysis

wt. % · EN 10095 ranges
C
≤0.10
Si
≤1.50
Mn
≤2.00
Cr
24.0–26.0
Ni
19.0–22.0
N
≤0.11

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Oxidation (scaling) resistance in air up to ≈ 1050 °C
  • High Cr and Ni; stable, fully austenitic structure
  • Low-carbon version of 310 (310S)
  • Good corrosion resistance in oxidising media (e.g. nitric acid)
  • Rm ≈ 500–700 MPa in the annealed condition (typical)
  • Sigma phase can form in prolonged service at 600–900 °C, lowering room-temperature toughness
  • Not hardenable by heat treatment; non-magnetic

02Applications

  • Furnace parts: grates, baskets, muffles, radiant tubes
  • Heat-treatment fixtures and carriers
  • Burner and combustion chamber parts
  • Recuperators and high-temperature heat exchangers
  • Hot-zone equipment in cement, petrochemical and power plants
  • Cryogenic equipment parts

03Delivery Condition

  • Solution annealed (max. 192 HB); bar, sheet, plate, tube, wire.

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →1050–1150 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 310S with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than 310S without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
  • Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
  • Detrimental phase testing for duplex steels (ASTM A923)

Supply status: Available on Request

Request 310S Quotation

Not sure if 310S is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote