2507 Super Duplex Stainless Steel

1.4410

Available on Request

  • EN1.4410
  • ENX2CrNiMoN25-7-4
  • UNSS32750
  • ASTMA182 F53 / A479
  • TicariSuper Duplex 2507

Super duplex (ferritic-austenitic) stainless steel (2507, UNS S32750, ASTM A182 F53) with 24–26 % chromium, 3–4.5 % molybdenum and 0.24–0.35 % nitrogen. Yield strength is at least 550 MPa and PREN is typically above 40, giving higher resistance than 2205 to pitting, crevice corrosion and stress corrosion cracking in seawater and hot chloride media. Supplied on request in the solution-annealed condition for offshore, seawater and chemical plant service.

Spectral Analysis

wt. % · EN 10088-3 ranges
C
≤0.030
Si
≤1.00
Mn
≤2.00
Cr
24.0–26.0
Ni
6.0–8.0
Mo
3.00–4.50
N
0.24–0.35

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rp0.2 ≥ 550 MPa, Rm ≥ 800 MPa (ASTM A182 F53 / A479)
  • High pitting and crevice corrosion resistance (PREN usually around 40 or higher; minimum set by the specification)
  • Resistance to chloride stress corrosion cracking
  • Higher strength and corrosion resistance than 2205
  • Magnetic
  • Service temperature −50 … +250 °C

02Applications

  • Offshore platforms and subsea equipment
  • Seawater cooling and firewater piping
  • Desalination plants, high-pressure lines
  • Pumps, valves, flanges and fittings (F53)
  • Chemical and petrochemical equipment
  • Hydraulic and instrumentation tubing

03Delivery Condition

  • Solution annealed (max. 310 HB, ASTM A182 F53); bar, plate, tube, forgings.

04Heat Treatment

Heat Treatment Steps

Soft annealingTemperatureTime →1040–1120 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as 2507 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 2507 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet
  • Forgings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 inspection certificate (upon request, third party)
  • Ultrasonic testing (e.g. EN 10308, ASTM A388), upon request
  • Intergranular corrosion testing (e.g. ASTM A262, EN ISO 3651-2)
  • Detrimental phase testing for duplex steels (ASTM A923)

Supply status: Available on Request

Request 2507 Quotation

Not sure if 2507 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote