Skip to content

M3:2 High Speed Steel

1.3344

  • EN1.3344
  • ENHS6-5-3
  • AISIM3:2

Mo-W high speed steel with vanadium raised to 2.7–3.2%, hardened to 64–66 HRC and more wear resistant than M2. Used for broaches, taps and hobs that cut abrasive materials; it is harder to grind than M2.

Spectral Analysis

wt. % · EN ISO 4957 ranges
C
1.17–1.27
Cr
3.80–4.50
Mo
4.70–5.20
V
2.70–3.20
W
5.90–6.70

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Higher wear resistance than M2
  • Good hot hardness
  • Moderate toughness
  • Grindability lower than M2
  • Heat treated to 64–66 HRC

02Applications

  • Broaches and taps
  • Milling cutters and hobs
  • Cutting tools for abrasive materials
  • Punching and cutting punches
  • High-performance drills

03Delivery Condition

  • Max. 269 HB, soft annealed (EN ISO 4957).

04Heat Treatment

Heat Treatment Steps

HardeningTemperatureTime →1. preheat~500 °C2. preheat~850 °C3. preheat~1050 °CAustenitise1180–1220 °C

Quench: 500–550 °C salt bath + air

TemperingTemperatureTime →1. temper540–570 °C2. temper540–570 °C3. temper540–570 °C
Stages and temperatures are typical values; soaking times depend on section size.

Tempering Diagram

0 °C → 64.5 HRC200 °C → 62.5 HRC300 °C → 61.5 HRC400 °C → 61 HRC500 °C → 63.5 HRC540 °C → 65.5 HRC560 °C → 66 HRC580 °C → 65 HRC600 °C → 63 HRC650 °C → 58 HRC0100200300400500600700505560657075Tempering temperature [°C]Hardness [HRC]1.3344Heat treatment: 1180–1220 °CQuench: 500–550 °C saltbath + air
Approximate hardness versus tempering temperature after hardening from the typical austenitising temperature.

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as M3:2 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than M3:2 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate (chemical analysis, delivery hardness)
  • EN 10204 3.2 inspection certificate (on request, third party)
  • Carbide distribution / microstructure evaluation (e.g. SEP 1615)
  • Decarburisation depth check
  • Ultrasonic testing, on request
Request M3:2 Quotation

Not sure if M3:2 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote