Skip to content

CuNi3Si Copper Alloy

CuNi3Si

  • ENCW112C
  • ENCuNi3Si1Mg
  • DIN2.0857
  • UNSC70250

CuNi3Si (CuNi3Si1Mg, CW112C) is a magnesium-bearing copper alloy hardened by nickel-silicon precipitates, giving about 180–230 HB and 40–50 % IACS conductivity. It is used where a beryllium-free material is required, e.g. electrode holders, mold cores and continuous casting components.

Spectral Analysis

wt. % · EN 12163 (CW112C) ranges
Cu
balance
Ni
2.60–4.50
Si
0.80–1.30
Mg
0.10–0.30

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Beryllium-free
  • Precipitation hardened: ~180–230 HB
  • Electrical conductivity ~40–50 % IACS
  • Good thermal conductivity
  • Good wear resistance and machinability

02Applications

  • Resistance welding electrode holders and arms
  • Plastic injection mold cores and cooling components
  • Connectors and spring contacts
  • Continuous casting mold components
  • High-strength conductive parts

03Delivery Condition

  • Precipitation-hardened rod and plate (TH04 / solution treated + aged).

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →900–950 °C
AgeingTemperatureTime →~475 °C
Stages and temperatures are typical values; soaking times depend on section size.

Ageing Diagram

0 °C → 85 HB400 °C → 170 HB450 °C → 205 HB475 °C → 215 HB500 °C → 210 HB550 °C → 185 HB600 °C → 145 HB01002003004005006005075100125150175200225250Ageing temperature [°C]Hardness [HB]CuNi3SiSolution treatment: 900–950 °C
Approximate hardness versus ageing temperature after solution treatment (0 °C = solution-treated condition).

Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.

05Is there a better material?

Grades in the same material family as CuNi3Si with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Round bar
  • Flat bar
  • Plate
  • Sheet / strip
  • Wire
  • Tube / hollow bar
  • Castings
  • Cut-to-size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 (on request, third party)
  • Chemical analysis (spectrometric) and PMI
  • Electrical conductivity measurement (% IACS / MS/m)
  • Hardness and tensile testing
Request CuNi3Si Quotation

Not sure if CuNi3Si is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote