Cu-OFE (C10100) Oxygen-Free Electronic Copper
Cu-OFE
Available on Request
- ENCW009A
- ENCu-OFE
- UNSC10100
- ASTMF68 (elektronik kalite)
Cu-OFE (CW009A, UNS C10100) is oxygen-free electronic copper with at least 99.99 % copper and no more than 5 ppm oxygen; its impurity limits, particularly for volatile elements, are much tighter than those of Cu-OF (C10200). It is used in vacuum, electron-tube, accelerator, RF and superconductor applications, and ASTM F68 microstructure testing can be specified for electronic grade.
Spectral Analysis
wt. % · ASTM B170 Grade 1 / B187 (C10100) ranges- Cu
- ≥99.99
- O
- ≤0.0005
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Electrical conductivity ≥ 101 % IACS (annealed)
- Thermal conductivity ≈ 390 W/m·K
- Immune to hydrogen embrittlement; can be annealed and brazed in hydrogen
- Low outgassing in high vacuum
- Very good cold and hot formability
- Low strength; hardness by cold work
02Applications
- Vacuum components and vacuum seals
- Electron tubes, magnetron and klystron parts
- Particle accelerator and RF cavity components
- Stabiliser in superconducting wire and cable
- High-power electronic and semiconductor parts
- Audio and signal conductors
03Delivery Condition
- Soft or cold worked; bar, flat, plate, tube, strip and wire (ASTM B187 / B152 / B75).
- Where electronic grade is required, ASTM F68 testing and conductivity are stated on the certificate.
04Heat Treatment
Heat Treatment Steps
Values are approximate and for information only; they vary with section size, heat and furnace conditions. Binding values are determined from the manufacturer’s data under laboratory conditions.
05Is there a better material?
Grades in the same material family as Cu-OFE with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
- CuCr1 Chromium Copper
Wear resistance: Very low → Low
Trade-off: Conductivity, Toughness
- CuCrZr Chromium Zirconium Copper
Wear resistance: Very low → Low
Trade-off: Conductivity, Toughness
Higher impact resistance (toughness)
Our list has no grade with higher impact resistance (toughness) than Cu-OFE without a marked trade-off in its other critical properties.
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights06Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Round bar
- Flat bar
- Plate
- Sheet / strip
- Wire
- Tube / hollow bar
- Castings
- Cut-to-size
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 (on request, third party)
- Chemical analysis (spectrometric) and PMI
- Electrical conductivity measurement (% IACS / MS/m)
- Hardness and tensile testing
Supply status: Available on Request
Request Cu-OFE QuotationNot sure if Cu-OFE is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.
Find the Right MaterialGrades in the Same Group
Back to GroupTechnical resources for this material
Have a material requirement?