Skip to content

7475 Aluminum Alloy

EN AW-7475

Available on Request

  • ENEN AW-7475
  • UNSA97475

EN AW-7475 (UNS A97475) is a high-purity derivative of 7075 with reduced iron and silicon for higher fracture toughness. It combines high strength with good fracture toughness and resistance to fatigue crack growth. Supplied to specification as T7351 / T7651 plate and sheet for fracture-critical aerospace parts.

Spectral Analysis

wt. % · EN 573-3 ranges
Al
balance
Zn
5.2–6.2
Mg
1.9–2.6
Cu
1.2–1.9
Cr
0.18–0.25
Si
≤0.10
Fe
≤0.12
Mn
≤0.06
Ti
≤0.06

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm ≈ 490 MPa, Rp0.2 ≈ 415 MPa (T7351 plate, typical)
  • Low Fe and Si: higher fracture toughness than 7075
  • Good resistance to fatigue crack growth
  • Stress corrosion and exfoliation resistance in T73 / T76 tempers
  • Density ≈ 2.81 g/cm³
  • Not suited to fusion welding

02Applications

  • Aerospace fuselage and wing skins
  • Bulkheads and wing root fittings
  • Fracture-critical structural parts
  • Defense and space structures

03Delivery Condition

  • T7351: overaged plate, stress relieved by stretching.
  • T7651: plate overaged for exfoliation resistance.
  • T61 / T761: sheet, on request.
  • Alclad sheet on request.
  • Standards: AMS, ASTM B209; customer specifications.

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →470–480 °C

Quench: Water

AgeingTemperatureTime →1. age~115 °C2. age~163 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are typical and vary with temper and thickness. Heat treatment is usually carried out by the mill to specification.

05Is there a better material?

Grades in the same material family as 7475 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 7475 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Our list has no grade with higher impact resistance (toughness) than 7475 without a marked trade-off in its other critical properties.

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Plate
  • Sheet
  • Round bar
  • Flat bar
  • Extrusions
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 (on request, third party)
  • Tensile and hardness testing (temper verification)
  • Temper verification by electrical conductivity (e.g. AMS 2658)
  • Ultrasonic testing (thick plate; e.g. ASTM B594 / AMS-STD-2154)

Supply status: Available on Request

Request 7475 Quotation

Not sure if 7475 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote