Skip to content

7050 Aluminum Alloy

EN AW-7050

Available on Request

  • ENEN AW-7050
  • ENAlZn6CuMgZr
  • UNSA97050

EN AW-7050 (AlZn6CuMgZr, UNS A97050) is a zirconium-bearing 7xxx-series aluminum alloy with low quench sensitivity. It retains high strength in thick sections, and in T74 / T7451 it balances stress corrosion and exfoliation resistance with fracture toughness. Supplied to specification as thick plate and forgings for aerospace.

Spectral Analysis

wt. % · EN 573-3 ranges
Al
balance
Zn
5.7–6.7
Cu
2.0–2.6
Mg
1.9–2.6
Zr
0.08–0.15
Si
≤0.12
Fe
≤0.15
Mn
≤0.10
Cr
≤0.04
Ti
≤0.06

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm ≈ 490–525 MPa, Rp0.2 ≈ 430–470 MPa (T7451 plate, thickness dependent, typical)
  • Low quench sensitivity; limited strength loss in thick sections
  • Good stress corrosion and exfoliation resistance (T74 / T76)
  • Good fracture toughness and fatigue strength
  • Density ≈ 2.83 g/cm³
  • Good machinability; not suited to fusion welding

02Applications

  • Aerospace fuselage frames and bulkheads
  • Wing spars and ribs
  • Monolithic parts machined from thick plate
  • Landing gear and structural forgings
  • Defense structural parts

03Delivery Condition

  • T7451: overaged plate, stress relieved by stretching.
  • T7452 / T74: forgings.
  • T76511 / T73511: extrusions, on request.
  • Standards: AMS (plate and forgings), ASTM B209 / B247; customer specifications.

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →471–482 °C

Quench: Water

AgeingTemperatureTime →1. age~120 °C2. age~170 °C
Stages and temperatures are typical values; soaking times depend on section size.

Values are typical and vary with temper and thickness. Heat treatment is usually carried out by the mill to specification.

05Is there a better material?

Grades in the same material family as 7050 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 7050 without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Plate
  • Sheet
  • Round bar
  • Flat bar
  • Extrusions
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 (on request, third party)
  • Tensile and hardness testing (temper verification)
  • Temper verification by electrical conductivity (e.g. AMS 2658)
  • Ultrasonic testing (thick plate; e.g. ASTM B594 / AMS-STD-2154)

Supply status: Available on Request

Request 7050 Quotation

Not sure if 7050 is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote