2017A Aluminum Alloy

EN AW-2017A

Available on Request

  • ENEN AW-2017A
  • ENAlCu4MgSi(A)
  • DIN3.1325
  • DINAlCuMg1

EN AW-2017A (AlCu4MgSi(A), former DIN AlCuMg1 / 3.1325) is the copper-bearing aluminum alloy known as duralumin, hardened by natural ageing. With good machinability and medium-to-high strength it is used for machine and machined parts. Usually supplied as T4 / T451 bar and plate.

Spectral Analysis

wt. % · EN 573-3 ranges
Al
balance
Cu
3.5–4.5
Mg
0.40–1.0
Mn
0.40–1.0
Si
0.20–0.8
Fe
≤0.7
Zn
≤0.25
Cr
≤0.10
Ti+Zr
≤0.25

Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties

  • Rm ≈ 390–420 MPa, Rp0.2 ≈ 250–270 MPa (T4 / T451, typical)
  • Hardness ≈ 105–115 HB
  • Good machinability; common on automatic lathes
  • Density ≈ 2.79 g/cm³
  • Limited corrosion resistance; anodising or a protective coating is recommended
  • Not suited to fusion welding

02Applications

  • Machine and fixture parts
  • Hydraulic and pneumatic components
  • Rivets and fasteners
  • Aerospace and defense machined parts
  • Automotive spare and tooling parts

03Delivery Condition

  • T4: solution treated and naturally aged; bar and extrusions.
  • T451: stress relieved by stretching; plate.
  • T3511 / T3: after drawing or straightening; bar, on request.
  • Standards: EN 573-3, EN 485, EN 754 / EN 755.

04Heat Treatment

Heat Treatment Steps

Solution treatmentTemperatureTime →~500 °C

Quench: Water

Stages and temperatures are typical values; soaking times depend on section size.

Values are typical and vary with product form and section. The ageing stage in the diagram represents natural ageing at room temperature.

05Is there a better material?

Grades in the same material family as 2017A with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.

Higher wear resistance

Our list has no grade with higher wear resistance than 2017A without a marked trade-off in its other critical properties.

Higher impact resistance (toughness)

Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.

For more information, browse our Technical Insights

06Move Metal Supply Options

Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.

Product forms

  • Plate
  • Sheet
  • Round bar
  • Flat bar
  • Extrusions
  • Forgings
  • Cut to size

Documents and testing

  • EN 10204 3.1 inspection certificate
  • EN 10204 3.2 (on request, third party)
  • Tensile and hardness testing (temper verification)
  • Temper verification by electrical conductivity (e.g. AMS 2658)
  • Ultrasonic testing (thick plate; e.g. ASTM B594 / AMS-STD-2154)

Supply status: Available on Request

Request 2017A Quotation

Not sure if 2017A is the right material for your application?

Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.

Find the Right Material

Grades in the Same Group

Back to Group

Technical resources for this material

Have a material requirement?

Send us your specification, drawing or RFQ. Our team will review the requirement and identify a suitable supply option.

Request a Quote