EN AW-5083 (AlMg4,5Mn0,7, UNS A95083) is a non-heat-treatable aluminum-magnesium alloy whose strength comes from magnesium and strain hardening. Its corrosion resistance in seawater and good weldability lead to use in ships, marine structures and pressure vessels. Supplied as plate and sheet in O / H111, H116 and H321 tempers.
Spectral Analysis
wt. % · EN 573-3 ranges- Al
- balance
- Mg
- 4.0–4.9
- Mn
- 0.40–1.0
- Cr
- 0.05–0.25
- Si
- ≤0.40
- Fe
- ≤0.40
- Cu
- ≤0.10
- Zn
- ≤0.25
- Ti
- ≤0.15
Typical ranges according to the standard, for information only. The analysis on the material certificate applies on delivery.

01Material Properties
- Rm ≈ 290 MPa, Rp0.2 ≈ 145 MPa (O / H111, typical)
- Rm ≈ 315–350 MPa, Rp0.2 ≈ 230 MPa (H116 / H321, typical)
- Good corrosion resistance in seawater and marine atmosphere
- Good weldability (5183 / 5356 filler wire)
- Retains toughness at low temperatures
- Sensitisation (intergranular corrosion) risk is reviewed for long service above 65 °C
02Applications
- Ship hulls, decks and superstructures
- Offshore and harbour structures
- Pressure vessels and LNG / cryogenic tanks
- Tanker and bulk trailer bodies
- Rail vehicle and transport structures
- Mold and fixture plates (cast / rolled plate)
03Delivery Condition
- O / H111: annealed; for forming.
- H116 / H321: stabilised marine tempers (ASTM B928).
- H32 / H34: strain-hardened and stabilised sheet.
- H112: hot-rolled plate.
- Standards: EN 485, ASTM B209 / B928; class society approval on request.
04Heat Treatment
Heat Treatment Steps
Values are typical and vary with temper and thickness.
05Is there a better material?
Grades in the same material family as 5083 with higher wear resistance and higher impact resistance (toughness); up to two suggestions under each heading. Which one fits depends on the application's priority requirement.
Higher wear resistance
Our list has no grade with higher wear resistance than 5083 without a marked trade-off in its other critical properties.
Higher impact resistance (toughness)
Our list has no grade with higher impact resistance (toughness) than 5083 without a marked trade-off in its other critical properties.
Suggestions are based on the critical property levels in our grade data; an improvement in one property may require a trade-off in another. The final selection must be made by technical evaluation against operating conditions, heat treatment and specification.
For more information, browse our Technical Insights06Move Metal Supply Options
Move Metal is not a producer; we source the grade to your specification through our international producer and supplier network. Dimensions, quantity, delivery condition and documentation requirements are reviewed together.
Product forms
- Plate
- Sheet
- Round bar
- Flat bar
- Extrusions
- Forgings
- Cut to size
Documents and testing
- EN 10204 3.1 inspection certificate
- EN 10204 3.2 (on request, third party)
- Tensile and hardness testing (temper verification)
- Temper verification by electrical conductivity (e.g. AMS 2658)
- Ultrasonic testing (thick plate; e.g. ASTM B594 / AMS-STD-2154)
Supply status: Available on Request
Request 5083 QuotationNot sure if 5083 is the right material for your application?
Evaluate candidate materials by application, operating conditions and priority properties with the Material Selection Guide.